ASTM A276 201 UNS S20100 Stainless steel

Prouduct name: ASTM A276 201 UNS S20100 Stainless steel

abstract: ASTM A276 201 UNS S20100 Stainless steel

Popular in these Categories: stainless steel

Contact: +86-0571-86628016

Chemistry Typical

Carbon: 0.15 max
Manganese: 5.50- 7.50 max
Phosphorus: .060 max
Sulfur: 0.030 max
Silicon: 0.75 max
Chromium: 18.00- 20.00 max
Nickel: 3.50- 5.50
Nitrogen: 0.25

Physical Properties

Density: 0.283 lbs/in³, 7.81 g/cm³

Electrical Resistivity: microhm-in, microhm-cm: 27.0 (68.5)

Specific Heat: BTU/lbs./°F (kJ/kg/K): 32-212°F (0-100°C):  0.12 (0.50)

Thermal Conductivity, BTU/hr/ft²/ft/°F (W/m/K):
At 212°F (100°C): 9.4 (16.2)
At 932°F (500°C): 12.4 (21.4)

Mean Coefficient of Thermal Expansion, in./in./ °F (µm/m/K)
32 – 212 °F (0 – 100 °C) 8.7 x 10-6 (15.7)
32 – 600 °F (0 – 315 °C) 9.7 x 10-6 (17.5)
32 – 1000 °F (0 – 538 °C) 10.2 x 10-6 (18.4)
32 – 1200 °F (0 – 649 °C) 10.5 x 10-6 (18.9)
32 – 1600 °F (0 – 871 °C) 11.3 x 10-6 (20.3)

Modulus of Elasticity, KSI (MPa)
28.6 x 10³(197 x 10³)

Magnetic Permeability, H= 200 Oersteds: Annealed: 1.02 max

Melting Range, °F (°C) – 2550 – 2650 (1399 – 1454)

Mechanical Properties at Room Temperature

Annealed Condition
Ultimate Tensile Strength: 95 KSI min (655 MPA min)
Yield Strength (0.2% Offset): 38 KSI min (260 MPA min)
Elongation: 40%min
Hardness: B95 max