UNS S31635 AISI 316Ti Stainless steel

This data sheet applies to stainless steel 316Ti / 1.4571 hot and cold rolled sheet and strip, semi-finished products, bars and rods, wire and sections as well as for seamless and welded tubes for pressure purposes.

Application

Construction encasement, doors, windows and armatures, off-shore modules, container and tubes for chemical tankers, warehouse and land transportation of chemicals, food and beverages, pharmacy, synthetic fibre, paper and textile plants and pressure vessels. Due to the Ti-alloy, resistance to intergranular corrosion is guaranteed after welding.

Chemical Compositions*

Element% Present (in product form)

C, H, PLTWTS
Carbon (C)0.080.080.080.08
Silicon (Si)1.001.001.001.00
Manganese (Mn)2.002.002.002.00
Phosphorous (P)0.0450.0450.0453)0.040
Sulfur (S)0.0151)0.0301)0.0153)0.0151)
Chromium (Cr)16.50 - 18.5016.50 - 18.5016.50 - 18.5016.50 - 18.50
Nickel (Ni)10.50 - 13.5010.50 - 13.502)10.50 - 13.5010.50 - 13.502)
Molybdenum (Mo)2.00 - 2.502.00 - 2.502.00 - 2.502.00 - 2.50
Titanium (Ti)5xC to 0705xC to 0705xC to 0705xC to 070
Iron (Fe)BalanceBalanceBalanceBalance

Mechanical properties (at room temperature in annealed condition)


Product Form

CHPLLTWTS
Thickness (mm) Max812751602502)6060
Yield StrengthRp0.2 N/mm22403)2203)2203)2004)2005)1906)1906)
Rp1.0 N/mm22703)2603)2603)2354)2355)2256)2256)
Tensile StrengthRm N/mm2540 - 6903)540 - 6903)520 - 6703)500 - 7004)500 - 7005)490 - 6906)490 - 6906)
Elongation min. in %
A1) %min (longitudinal)---40-3535
A1) %min (transverse)404040-303030
Impact Energy (ISO-V) ≥ 10mm thickJmin (longitudinal)-9090100-100100
Jmin (transverse)-60600606060

Reference data on some physical properties

Density at 20°C kg/m38.0
Modulus of Elasticity kN/mm2 at20°C200
200°C186
400°C172
500°C165
Thermal Conductivity W/m K at 20°C15
Specific Thermal Capacity at 20°C J/kg K500
Electrical Resistivity at 20°C Ω mm2 /m0.75

Coefficient of linear thermal expansion 10-6 K-1 between 20°C and

100°C16.5
200°C17.5
300°C18.0
400°C18.5
500°C19.0

 